The idea
Forming changes a part’s shape by deforming it plastically, without removing material. makes sheet, plate and sections; hammers or presses billets into strong parts; pushes metal through a die; sheet-metal work bends, stretches and draws thin sheet. allows big changes with low force; gives accuracy, finish and extra strength.
Everyday intuition
Rolling pastry with a rolling pin: each pass makes it thinner, longer and a little wider. Squeeze too much in one pass and the pin just skids — exactly like rolls that cannot grip a strip when the draft is too large.
How it works
- Plastic flow. The stress must exceed the flow stress; volume stays the same, so a thinner strip gets longer and faster.
- Hot or cold. Above the recrystallisation temperature (about 0.6 of the melting point in kelvin) new grains form as you work, so the metal stays soft; below it, it work-hardens.
- Rolling. Draft d = h₀ − h_f; the rolls only grip the strip if d ≤ μ²R. Roll force ≈ flow stress × width × contact length √(Rd).
- Forging. Open-die (simple shapes, big parts) or closed-die (near-net shape, flash squeezed out). Grain flow follows the part’s outline, which helps fatigue strength.
- Extrusion and drawing. Extrusion pushes through a die (window frames, heat sinks); drawing pulls through a die (wire, tube).
- Sheet metal. Shearing and blanking, bending (watch and the minimum bend radius), deep drawing (cans, sinks) and stretch forming.
It leaves thinner and faster; contact length is about √(R d).
Key formulas
Flat rolling — draft, strain and force:
- entry and exit thickness mm
- roll–strip friction coefficient none
- roll radius mm
- average flow stress MPa
- strip width mm
Worked example
Where it is used
- Steel sheet for car bodies: hot rolled, then cold rolled and pressed into panels.
- Crankshafts and connecting rods: closed-die forged for fatigue strength.
- Aluminium window frames and heat sinks: extruded.
- Drinks cans: deep drawn and ironed from a disc of sheet.
Common misconceptions
Self-check
Check Why do rolls fail to grip a strip when the draft is too large?
Show answer
The friction force pulling the strip in is not enough; the largest draft is about μ²R.
Check What happens to a strip's speed as it leaves the rolls thinner?
Show answer
It speeds up, since volume flow h·w·v is constant.
Check Why do forged crankshafts resist fatigue better than machined ones from bar?
Show answer
Forged grain flow follows the shape instead of being cut across at the fillets.