Corrosion
Why metals corrode, galvanic corrosion between different metals, passivation, and the main ways to prevent corrosion.
0 deeper section(s) hidden.
On this page
The idea
is the slow destruction of a metal by reaction with its surroundings, usually water and oxygen. It is electrochemical: at one place the metal dissolves and releases electrons, which are used up somewhere else. When two different metals touch in water, the more active one corrodes much faster: . Engineers prevent it with barriers, , such as , and good design.
Everyday intuition
An iron gate rusts first at the bottom where water collects. A bicycle chain left outside turns orange. Ships carry zinc blocks on their hulls that slowly disappear while protecting the steel.
How it works
- Two half-reactions (explained below): the metal is oxidised at the anode, and the electrons are used up at the cathode.
- An electrolyte is needed. Dry air causes little corrosion; salty water causes a lot.
- Galvanic series. When two metals touch in water, the more active one (zinc, aluminium, magnesium) becomes the anode and corrodes; the more noble one (stainless steel, copper) is protected. A small anode joined to a large cathode corrodes very fast.
- Local attack — pitting, crevice corrosion and stress corrosion cracking — can cause failures with little visible metal loss.
- Prevention combines material choice, coatings, cathodic protection, insulating dissimilar metals, avoiding water traps, and a corrosion allowance.
In more detail
Corrosion involves two separate processes or half-reactions, oxidation and reduction. Oxidation is the reaction that consumes metal atoms when they corrode, releasing electrons. These electrons are used up in the reduction reaction.
When a metal corrodes in solution, the two halves of the reaction can be separated by large distances. This is unlike oxidation in air, when one reaction occurs at the surface of the film and the other at the surface of the metal, meaning that the reaction sites are always close to each other. In fact, in aqueous solution the reaction separation can be very large and as long as there is both electronic and electrolytic contact between the anodic and cathodic sites, corrosion will occur regardless of separation of the half-reactions.
Another effect that limits the rate of corrosion is passivation. If the potential of an electrode is raised above some passivation potential, a passive product may become favourable forming a layer on the surface of the anode. In this case, the rate of corrosion can be much reduced. This is characterised by the value of log (i) peaking at a critical current density, before falling to some lower value.
It is possible to deliberately drive the reaction into the regime in which a passive layer forms. This technique is used in the process known as anodising in which thick oxide layers are developed on aluminium components.
There are several ways kinetics can be employed to reduce or prevent corrosion.
Barriers and coatings
A barrier can be employed to prevent the electrolyte coming into contact with the metal.
Tin is the usual barrier, as it does not react in most aqueous solutions. It is used in food cans and has the useful property that if the barrier fails, then the steel in the can corrodes. If zinc were used instead it would begin to act as a sacrificial anode should the barrier fail. This would protect the steel but the distinct disadvantage is that hydrogen is evolved at the steel cathode and if it were to build up inside a closed container an explosive situation could arise.
Other inert metals may be used as barriers, as can polymers, ceramics and paint.
Cathodic protection
Cathodic protection lowers the electrical potential of the metal so that it becomes the cathode and stops corroding. It is done with an impressed current (electrons supplied from an external power source) or with a sacrificial anode: a more active metal, such as zinc, attached to the structure so that it corrodes instead.
Electrons flow through the metal; ions move through the water.
Key formulas
Corrosion allowance:
- extra wall thickness mm
- uniform corrosion rate mm/year
- design life years
Worked example
Where it is used
- Ships, piers and offshore platforms: sacrificial anodes, coatings and impressed-current systems.
- Buried pipelines: coatings plus cathodic protection.
- Car bodies: galvanized steel and paint layers.
- Aluminium parts: anodising thickens the protective oxide.
Common misconceptions
Self-check
Check Why do galvanized nails keep protecting the steel even where the zinc is scratched?
Show answer
Zinc is more active than steel, so it corrodes sacrificially and protects the exposed steel nearby.
Check A boat has a bronze propeller and a steel shaft. Which part is at risk, and how is it protected?
Show answer
The steel, the more active metal. A zinc or aluminium sacrificial anode is fitted so it corrodes first.
Check A tank corrodes at 0.05 mm per year. What allowance is needed for 40 years?
Show answer
mm.