Module 2 · Strength of materials

Fatigue

How parts break after millions of small, repeated loads that would never break them once — the most common way machine parts fail.

Notes
On this page
  1. The idea
  2. Everyday intuition
  3. How it works
  4. Key formulas
  5. Worked example
  6. Where it is used
  7. Common misconceptions
  8. Self-check

The idea

is failure under a load that is applied and removed, or reversed, many times. Each cycle is far below the stress needed to break the part in one go, but a tiny crack starts at a weak spot and grows a little with every cycle until the remaining metal snaps. Fatigue causes a large share of mechanical failures in shafts, springs, bolts, axles and aircraft structures.

Everyday intuition

Bend a paper clip back and forth: it does not break on the first bend, but after a dozen or so it snaps. A wire coat hanger, a ring-pull on a can and a cracked phone charging cable all fail this way. The load was never large; it was repeated.

How it works

  1. Crack initiation. Repeated stress causes tiny slip movements at the surface, usually where stress is concentrated: a scratch, a corner, a thread, a weld toe or a corrosion pit. After many cycles a microscopic crack forms.
  2. Crack growth. Each cycle opens and closes the crack tip and pushes it forward a tiny amount. The crack grows across the section, leaving a smooth surface. Pauses and changes in loading leave curved pointing back to the origin.
  3. Final fracture. When the remaining section is too small to carry the peak load, it breaks suddenly in one cycle, leaving a rough, often bright surface.
  4. The S–N curve. Testing many specimens at different and counting cycles to failure gives the . Lower stress means longer life.
  5. Endurance limit — sometimes. Steels and titanium alloys show an : below a certain amplitude, test specimens do not fail however many cycles are applied. Aluminium and copper alloys show no such limit; they eventually fail at any repeated stress, so designers use a fatigue strength at a stated number of cycles.
  6. Mean stress matters. A cycle that swings between two tensile values is more damaging than one that swings equally about zero with the same amplitude. Higher shortens life.
Cycles to failure N (log scale) Stress amplitude S 10³10⁴10⁵10⁶10⁷10⁸ steel endurance limit aluminium

Aluminium has no flat region: it keeps falling.

Schematic S–N curves. Steel levels off at an endurance limit; aluminium keeps falling. S–N curves: with and without an endurance limit. Original diagram drawn for this site. Schematic, not to scale. Tap labelled parts for an explanation.
S–N curves: with and without an endurance limit
Close-up of the broken end of an aluminium bicycle pedal arm. A smooth dark region with curved bands near the lower edge is where the fatigue crack grew slowly; the rest of the face is rough and bright where the arm finally snapped. An inset shows the whole arm.
Fatigue failure of an aluminium bicycle pedal arm. The dark, smooth region with curved beach marks is where the crack grew slowly over many pedal strokes; the bright, rough region is the final sudden fracture. “Pedalarm Bruch” by Lokilech. CC BY-SA 3.0. Source. Changes: Resized to 1200 px wide and converted to WebP.
End view of a fractured bolt. A large smooth, flat region covers most of the face, with a narrow rough band along the top edge where the remaining metal tore apart.
Fatigue fracture of a high-strength bolt: a large smooth crack-growth region and a narrow rough band of final overload. “Bolt-fatigue-fracture” by Wang Hui-li, Qin Si-feng (from “High-Strength Bolt Corrosion Fatigue Life Model and Application”, The Scientific World Journal, doi:10.1155/2014/567318). CC BY 4.0. Source. Changes: Converted to WebP.

Key formulas

For a load that cycles between σmax⁡\sigma_{\max} and σmin⁡\sigma_{\min}:

σa=σmax⁡−σmin⁡2σm=σmax⁡+σmin⁡2R=σmin⁡σmax⁡\sigma_a = \frac{\sigma_{\max} - \sigma_{\min}}{2} \qquad \sigma_m = \frac{\sigma_{\max} + \sigma_{\min}}{2} \qquad R = \frac{\sigma_{\min}}{\sigma_{\max}}

A common first estimate of the endurance limit of a polished steel test specimen:

Se′≈0.5 σu(up to about 290 MPa)S_e' \approx 0.5\,\sigma_u \quad (\text{up to about } 290\ \text{MPa})
σa\sigma_a
stress amplitude (half the range) Pa
σm\sigma_m
mean stress Pa
RR
stress ratio (−1 for fully reversed loading) none
Se′S_e^{\prime}
endurance limit of a smooth laboratory specimen Pa
σu\sigma_u
ultimate tensile strength Pa

Worked example

Where it is used

  • Axles, crankshafts and drive shafts rotate, so every revolution is one cycle of bending.
  • Aircraft are inspected at intervals set by fatigue crack-growth calculations.
  • Springs, connecting rods and turbine blades are designed against millions or billions of cycles.
  • Welded structures (bridges, cranes, offshore platforms) follow fatigue classes for each weld detail in design codes.
  • Shot peening, rolling threads and polishing are used in factories to improve fatigue life by putting the surface into compression or removing scratches.

Common misconceptions

Animated explanation of fatigue failure, crack growth and S–N curves. Video: “Understanding Fatigue Failure and S-N Curves” by The Efficient Engineer, embedded from YouTube. Watch on YouTube if the player does not load.

Self-check

Check A spring's stress cycles between 100 MPa and 300 MPa. Find the stress amplitude, mean stress and R.

Show answer

σa=(300−100)/2=100 MPa\sigma_a = (300 - 100)/2 = 100\ \text{MPa}; σm=(300+100)/2=200 MPa\sigma_m = (300 + 100)/2 = 200\ \text{MPa}; R=100/300=0.33R = 100/300 = 0.33.

Check On a fatigue fracture surface, how can you tell where the crack started?

Show answer

Beach marks form curved bands around the origin, like ripples. The origin is at the centre of those curves, usually at the surface and often at a notch or scratch. The final fracture zone is rough and lies on the opposite side.

Check Why might an aluminium aircraft part have a fixed service life in flights, even if it shows no cracks?

Show answer

Aluminium alloys have no endurance limit, so every load cycle uses up some of their fatigue life. The part is retired or inspected after a set number of cycles to stay safely within its tested life.

My notes

Private to this browser. Select any text above to highlight it.