Module 3 · Materials science · Summary
Module 3 summary: materials science
The whole module on one printable page.
On this page
Big ideas
- Properties come from structure. Atoms, bonding, crystal arrangement and grain size set stiffness, strength, ductility and conductivity.
- Metals are crystals. BCC, FCC and HCP arrangements; dislocations let metals deform plastically, which is why they are ductile.
- Alloying and heat treatment strengthen metals by getting in the way of dislocations.
- The iron–carbon diagram explains steel: under about 2% carbon is steel, above is cast iron; 0.76% C at about 727 °C is the eutectoid point where austenite turns to pearlite.
- Quench hard, temper tough. Quenching makes hard, brittle martensite; tempering trades some hardness for toughness.
- Polymers are long chains: thermoplastics soften on heating, thermosets do not, elastomers stretch.
- Ceramics are hard, stiff and heat-resistant but brittle: cracks do not blunt.
- Composites put stiff fibres in a tough matrix and are strongest along the fibres.
- Corrosion is electrochemical; stop it by barrier, sacrificial or passive protection, and avoid dissimilar metals in contact.
- Selection: screen by constraints, rank by a material index such as E/ρ or √E/ρ, then check the details.
Formula sheet
| Formula | Notes | |
|---|---|---|
| Elastic strain | Brittle ceramics stay elastic up to fracture. | |
| Rule of mixtures, along the fibres | Upper bound; loading along the fibres. | |
| Rule of mixtures, across the fibres | Lower bound; loading across the fibres. | |
| Density of a composite | Volume-weighted average. | |
| Corrosion allowance | Uniform corrosion only; r from data for the actual environment. | |
| Atomic packing factor | FCC π/(3√2) ≈ 0.74; BCC π√3/8 ≈ 0.68. | |
| Heat to raise a temperature | No phase change; c roughly constant. | |
| Lever rule | C₀ overall composition; Cα, Cβ phase compositions at that temperature. | |
| Specific stiffness and strength | Per unit mass. Steel and aluminium have almost the same E/ρ. | |
| Thermal expansion of a bar | α coefficient of thermal expansion (1/K). | |
| Material index, light stiff tie | Mass for equal stiffness ∝ 1/M. | |
| Material index, light stiff beam | Beam depth free to change. E in GPa, ρ in Mg/m³. | |
| Mass of an alloying element | w_i mass fraction (wt% ÷ 100). | |
| Equal bending stiffness (rectangular beam, same width) | Same load, span and deflection. |
Typical values used in this module
| Material | E (GPa) | Density (kg/m³) | Source |
|---|---|---|---|
| Structural steel (A36) | 200 | 7800 | Wikipedia, “A36 steel” |
| Aluminium alloy 6061-T6 | 69 | 2700 | Wikipedia, “6061 aluminium alloy”, “Aluminium” |
| Polystyrene | 3.0–3.6 | 960–1050 | Wikipedia, “Polystyrene” |
Checklist for any materials question
- What must the part do (load, temperature, environment, life)?
- Which property limits it: stiffness, strength, toughness, hardness, conductivity, corrosion?
- How does structure (crystal, grains, alloying, heat treatment, fibres) control that property?
- Compare candidates per unit mass or per unit cost, not just absolute values.
- Check the trade-off: harder usually means more brittle; stiffer fibres mean direction-dependent properties.
My notes
Private to this browser. Select any text above to highlight it.
This browser is blocking storage, so progress and notes will reset when you leave.