Casting
Pouring molten metal into a mould — sand, die and investment casting, shrinkage, risers and Chvorinov's rule.
0 deeper section(s) hidden.
On this page
The idea
makes a part by pouring molten metal into a cavity shaped like the part and letting it freeze. It can make almost any shape, from a ring to a ship’s propeller, but metal shrinks as it cools, so the mould is made oversize and a feeds the casting while it freezes. says the solidification time grows with (volume ÷ surface area)².
Everyday intuition
Ice cubes and a big block of ice in the same freezer: the cubes, with lots of surface for their size, freeze first. In a casting the thin parts freeze first and the chunky parts last, so the last place to freeze must be a riser, not the part.
How it works
- Make a pattern — a copy of the part, a little oversize for shrinkage, with draft angles so it can be pulled out of the sand.
- Make the mould. In sand is packed round the pattern in two halves (cope and drag); cores of sand form internal holes.
- Gating. A pouring cup, sprue and runners lead metal smoothly into the cavity; risers sit next to the thickest sections.
- Pour and freeze. Thin sections freeze first. Chvorinov: t = C(V/A)², so a riser with a larger V/A freezes after the section it feeds.
- Shake out, cut off risers and gates, clean and machine the faces that must be accurate.
- Other processes. (aluminium and zinc under pressure in steel dies: fast, accurate, costly tooling); (lost wax: fine detail, turbine blades, jewellery); centrifugal casting (pipes); permanent-mould casting.
- Defects. Shrinkage cavities (poor feeding), gas porosity, cold shuts (two streams that do not fuse), misruns (metal froze before filling), hot tears.
The riser freezes last and feeds the casting as it shrinks.
Key formulas
Chvorinov’s rule (solidification time):
- solidification time s
- casting volume mm³
- cooling surface area mm²
- mould constant s/mm²
Worked example
Where it is used
- Engine blocks and cylinder heads: sand or permanent-mould cast iron and aluminium.
- Pump and valve bodies: complex internal passages from sand cores.
- Turbine blades: investment cast, some as single crystals.
- Phone and laptop frames, gearbox housings: high-pressure die casting.
Common misconceptions
Self-check
Check Why must a riser freeze after the casting?
Show answer
So it can keep feeding liquid metal into the casting as it shrinks; otherwise a shrinkage cavity forms.
Check Name one advantage and one drawback of die casting compared with sand casting.
Show answer
Advantage — fast, accurate, smooth; drawback — expensive dies, mainly low-melting alloys.
Check A cube of side 100 mm has V/A of 16.7 mm. What is the V/A of a cube of side 50 mm?
Show answer
8.33 mm (V/A = side/6), so it freezes about four times faster.