Module 3 · Materials science

The iron–carbon diagram

The map of steel — how carbon content and temperature decide whether iron is ferrite, austenite or pearlite — and how to read it with the lever rule.

Notes
On this page
  1. The idea
  2. Everyday intuition
  3. How it works
  4. Key formulas
  5. Worked example
  6. Where it is used
  7. Common misconceptions
  8. Self-check

The idea

A shows which are stable at each temperature and composition for slow cooling. For steel the key map is the iron–carbon diagram. Iron has two solid forms: (BCC, holds almost no carbon) and (FCC, stable when hot, holds much more). When austenite with 0.76% carbon cools slowly through about 727 °C it becomes , fine layers of ferrite and hard — the point. Below about 2% carbon the alloy is steel; above, cast iron.

Everyday intuition

Picture a warm sponge (austenite) holding plenty of water (carbon). As it cools it turns into a sponge that holds almost none (ferrite), so the water is squeezed out into separate pockets (cementite layers). How slowly you cool decides how neatly the pockets form.

How it works

  1. Axes. Carbon content (wt%) along the bottom, temperature up the side. Steels use the part from 0 to about 2% carbon.
  2. Austenite region. Heated high enough, a steel is a single FCC phase with all its carbon dissolved.
  3. Eutectoid point. At 0.76% C and about 727 °C, austenite turns entirely into pearlite on slow cooling. (Sources quote 723–727 °C.)
  4. Below 0.76% C (most structural steels): soft ferrite forms first, then the remaining austenite becomes pearlite. From 0.76 to about 2% C (tool steels): cementite forms first, then pearlite — harder and more brittle.
  5. Cast irons (over about 2% C) pass through the eutectic at 4.3% C and 1147 °C, so they melt at much lower temperatures than steel.
  6. Only slow cooling. Quenching makes martensite, which is not on this diagram (next topic).
  7. How much of each phase? Use the lever rule, explained in the adapted text below.

In more detail

If an alloy consists of more than one phase, the amount of each phase present can be found by applying the lever rule to the phase diagram.

The lever rule can be explained by considering a simple balance. The composition of the alloy is represented by the fulcrum, and the compositions of the two phases by the ends of a bar. The proportions of the phases present are determined by the weights needed to balance the system.

A horizontal bar balanced on a pivot. The pivot is at the alloy's composition C, and the two ends are at the compositions C1 and C2 of the two phases; the weights needed to balance the bar represent the amounts of each phase.
The lever rule as a balance: the alloy composition is the pivot; the two phase compositions are the ends. “The lever rule (figure)” by DoITPoMS, University of Cambridge. CC BY-NC-SA 4.0. Source. Changes: Converted from GIF to WebP; no other changes.

So,

fraction of phase 1 = (C2 - C) / (C2 - C1)

and,

fraction of phase 2 = (C - C1) / (C2 - C1).

Iron–carbon diagram (simplified, slow cooling) carbon content (wt%) temperature (°C) 0 0.76 2.1 4.3 727 1147 austenite γ liquid eutectoid 0.76%, 727 °C eutectic 4.3% ferrite + pearlite pearlite + Fe₃C steel cast iron

Steel below about 2% carbon; cast iron above.

A simplified iron–carbon diagram for steels and cast irons. Tap the regions for details. Simplified iron–carbon phase diagram. Original diagram drawn for this site. Tap labelled parts for an explanation.
Simplified iron–carbon phase diagram
Microscope image of slowly cooled steel: wavy stripes of light and dark layers (pearlite) filling grains separated by thin boundaries.
Pearlite under a microscope: alternating thin layers of soft ferrite and hard cementite, formed when steel cools slowly through the eutectoid temperature. “Pearlite1” by Edward Pleshakov. Public domain. Source. Changes: Resized and converted to WebP.

Key formulas

Lever rule:

fβ=C0−CαCβ−Cαfα=1−fβf_\beta = \dfrac{C_0 - C_\alpha}{C_\beta - C_\alpha} \qquad f_\alpha = 1 - f_\beta
C0C_0
overall composition wt%
Cα, CβC_\alpha,\ C_\beta
compositions of the two phases wt%
fα, fβf_\alpha,\ f_\beta
mass fractions of the phases none

Worked example

Where it is used

  • Choosing a steel grade: low-carbon for welding and pressing, medium-carbon for shafts and gears, high-carbon for springs and cutting tools.
  • Planning heat treatment: the austenite region sets how hot to heat before hardening or normalising.
  • Welding: the heat-affected zone passes through these changes, which is why some steels need preheating.

Common misconceptions

An NPTEL lecture working through the iron–carbon phase diagram in detail (about 55 minutes). Video: “Mod-01 Lec-23 Iron-Carbon Phase Diagram” by nptelhrd, embedded from YouTube. Watch on YouTube if the player does not load.

Self-check

Check What forms when a 0.76% carbon steel cools slowly through 727 °C?

Show answer

Pearlite only: all the austenite becomes layers of ferrite and cementite.

Check What fraction of a 0.2% carbon steel is pearlite just below 727 °C?

Show answer

(0.20−0.02)/(0.76−0.02)=0.24(0.20 - 0.02)/(0.76 - 0.02) = 0.24 — mostly ferrite, so soft and ductile.

Check Why does austenite dissolve more carbon than ferrite?

Show answer

FCC austenite has larger gaps between its iron atoms than BCC ferrite.

My notes

Private to this browser. Select any text above to highlight it.

↑ ↓ move Enter open Esc close